Specifications & CoA
TEM Diameter | Size Distribution (CV) | Example Certificate of Analysis(How do I read this?) |
---|---|---|
5 nm ± 1 nm | ≤ 18% | Download Example CoA |
10 nm ± 2 nm | ≤ 12% | Download Example CoA |
20 nm ± 3 nm | ≤ 15% | Download Example CoA |
30 nm ± 3 nm | ≤ 15% | Download Example CoA |
40 nm ± 4 nm | ≤ 15% | Download Example CoA |
50 nm ± 4 nm | ≤ 15% | Download Example CoA |
60 nm ± 4 nm | ≤ 15% | Download Example CoA |
70 nm ± 5 nm | ≤ 15% | Download Example CoA |
80 nm ± 5 nm | ≤ 15% | Download Example CoA |
100 nm ± 5 nm | ≤ 15% | Download Example CoA |
Note: approximate ranges below are dependent on diameter
- Endotoxin Concentration: < 2.5 EU/mL (< 5.0 EU/mL for ≤ 20 nm sizes)
- Hydrodynamic diameter (DLS): TEM diameter plus 2 to 12 nm
- Zeta potential: –15 to –60 mV
- pH of solution: 5.3 to 7.0
- Particle surface: Sodium Citrate
- Solvent: USP Purified Water
- Peak wavelength (λmax): 515 to 560 nm
Molarity and particle concentration table ❯
More Info & Documentation
- Purchasing Information
- Storage & Handling
- UV-Vis QC Check Excel Template for monitoring particle stability over time
- Safety Data Sheet (SDS)
nanoComposix University
- Learn more about gold nanoparticles
- Learn more about citrate
- Learn more about BioPure
- Measuring UV-Vis for nanoparticle solutions
- FAQ
Peer-Reviewed Papers
- Gold and silver nanoparticle interactions with human proteins: Impact and implications in biocorona formation
- Analysis of Surface Bound Organic Ligands on Gold Nanomaterials Using Direct Sample Analysis-Time of Flight Mass Spectrometry
- Programming colloidal bonding using DNA strand-displacement circuitry (Supplementary Information)
AUCB 5nm 10nm 15nm 20nm 30nm 40nm 50nm 60nm 80nm 100nm
nanocomposix的动态光散射(DLS)纳米颗粒分析动态光散射(DLS)可测量溶液中纳米颗粒的流体动力学直径,并提供有关溶液中纳米颗粒聚集状态的信息。在nanoComposix上,DLS测量是在Malvern Zetasizer Nano ZS仪器上进行的,该仪器配备工作在632.8 nm的HeNe激光器和173度的散射检测器。